Why did the SMT pad fall off easily when soldering the PCB boards?

I am a buyer in a telecom company. Recently, an important order of SMT PCBA is delayed due to insophiscated production of a supplier. I am thinking about replace it and just very puzzled about how did their SMT pad fall off easily when soldering the PCB boards. That slows down the whole process.

I’m guessing that this was a hand-soldering operation. Most likely, the iron was too hot, or it was held on the pad too long, or both. If the latter, there may have been insufficient flux to enable good heat conduction into the joint, so the operator was forced to keep the iron in place longer than should have been necessary.

The epoxy in the PCB gets distinctly soft above the glass transition temperature(Tg). Guess what? All normal soldering operations happen above the glass transition temperature!

ItemTemp.
Traditional FR4 boardsTg: 135C
modern boards for lead-free soldering processesTg: 170C
Solder melting temperatures for eutectic Tin-Lead (Sn63)183C
melting temperatures lead-free solders (SAC305)217C
oldering iron temperature above the liquidus130C

Facing this problem in soldering operation, all we need to do is making it so fast that there isn’t time for the epoxy to go soft, and that there is no time for the copper pad to lose all adhesion.

And, greater soldering technique should allow the flux to do the work of heat conduction. The soldering iron tip even does not, in fact, touch either component or PCB.

 

In real life, we almost all do allow such contact, but we take care not to exert pressure while doing so. Because undue pressure is what causes pads to fall off if the temperature has gotten too high!

 

In addition, tip condition may be the second factors. Tips, which are badly tinned, stop the heat transfer to the joint. Subsequently, many operators have to increase the iron temperature and press the iron into the board hard enough to do push-ups, causing SMT pad falling with ease.

#PCB Assembly #SMT PCB Assembly #PCB Manufacturing

https://www.youtu.be/kX4gCs9szeA?si=F4ehyNfLGBTr8GyG

Oliver Smith

Oliver Smith

Oliver is an experienced electronics engineer skilled in PCB design, analog circuits, embedded systems, and prototyping. His deep knowledge spans schematic capture, firmware coding, simulation, layout, testing, and troubleshooting. Oliver excels at taking projects from concept to mass production using his electrical design talents and mechanical aptitude.
Oliver Smith

Oliver Smith

Oliver is an experienced electronics engineer skilled in PCB design, analog circuits, embedded systems, and prototyping. His deep knowledge spans schematic capture, firmware coding, simulation, layout, testing, and troubleshooting. Oliver excels at taking projects from concept to mass production using his electrical design talents and mechanical aptitude.

What Others Are Asking

What will be the role of a copper layer in a metal core PCB in thermal dissipation?

In the design of a power electronic PCB, I want to use a metal PCB for heat dissipation of a TO-220 package MOSFET. To do that I want to mount metal PCB on the MOSFET with the use of thermal paste and screw exactly like we do when we use heatsink for the same package. Should I leave the copper of PCB between MOSFET surface and dielectric of PCB or remove the copper surface and leave only the dielectric opening?

Who controls the process control block(PCB)?

Recently, I have learnt about kernel and find a question that who controls the process control block(PCB)?The kernel or the process itself? Does it differ in different platform (windows/Linux)? So far, I know PCB is controlled in hardware, but I can’t get to the right answer.

Read Detailed Advice From Blog Articles

Scroll to Top